Product Description
The basic process of continuous casting and rolling is: aluminum ingot → melting furnace → static furnace → degassing → filtering → casting nozzle → casting and rolling → guide roller → coiler.
Features
The molten aluminum is cast and rolled into slabs with a thickness of 6--10mm and a width of 450--2100mm and coiled to provide billets for the cold rolling mill. In this way, in the production process of aluminum sheet and strip, processes such as ingot casting, heating, hot rolling, and billeting are omitted, which shortens the technological process of aluminum sheet and strip production, reduces metal burning loss in the production process, saves energy, and saves energy. It can easily realize the continuous production of aluminum sheet and strip.
Technical Patameters
| Aluminum alloy | 1000,3000,8000 |
| Product thickness | 6-10 mm |
| Max.rolling force | 6000-25000 Kn |
| Product width | 800--1600 mm 801- |
| Length of roll surface | 1000-1850 mm |
| Dia.of casting roll | 600-1000mm |
| Max.coil weight | max 15000 Kg |
| Rolling speed | 800-5000 mm/min |
| Electric control system | Siemens |
Aluminum Casting and Rolling Mill
The molten aluminum is cast and rolled into slabs with a thickness of 6--10mm and a width of 450--2100mm and coiled to provide billets for the cold rolling mill.